When a coated part underperforms, the investigation almost always starts at the coating: layer design, deposition process, thickness errors. A substantial share of those investigations end somewhere earlier in the process — at the substrate. A coating is a thin film sitting on a piece of polished glass, and the film inherits the glass's history.

Striae: the invisible gradient
Striae are refractive-index inhomogeneities inside the glass, produced during melting and annealing. They are invisible to casual inspection, but a wavefront measurement shows them immediately: transmitted wavefront error that cannot be traced to surface figure is usually striae.
For a filter or mirror used in imaging or laser work, striae are a permanent defect that no coating can remove. They matter most in transmission-heavy applications — wavefront-critical relay optics, interferometer components, high-power laser paths — where the beam travels through the thickness. A part that is specified at λ/10 transmitted wavefront needs substrate material with a striae grade to match; the surface can be perfect and the wavefront still fail through the bulk.
The practical point for buyers: transmitted wavefront is a system specification that spans surface figure, surface quality, material homogeneity and coating stress. Asking for it by number, rather than specifying surface flatness alone, is what forces the whole chain to be adequate.
Bubbles and inclusions
Bubbles are evaluated per glass grade with defined size and count limits per 100 cm³. The relevant question is not "does the glass have bubbles" — all melt-produced glass does — but whether bubbles fall inside the used aperture at a size that matters. In an imaging path, a single bubble near the focal region is a visible artefact; the same bubble in a mounting border is irrelevant. Drawings that say "no bubbles" get expensive quotations; drawings that say "no bubbles larger than 0.1 mm within the 8 mm central aperture" get parts that work.
Polish quality is a coating variable
Coating adheres to the top few nanometres of the surface, and that region's condition is set by polishing and cleaning. Sub-surface damage left by loose-abrasive lapping, polishing residue, and cleaning-agent traces all change what the coating sees. In practice this shows up as:
- Adhesion failures that occur at scattered points rather than uniformly — the classic signature of localised surface contamination.
- Scatter that increases with coating roughness measurements on poorly polished substrates.
- LIDT reductions, because damage begins at defects, and defects live at the surface.
A coating house receiving unknown substrates will quote accordingly. One receiving substrates with a documented polish process — pitch or deterministic, known final cleaning — can push the same coating design to better results.
Cleaning is the last polish step
Between polishing and coating, the substrate passes through cleaning, and cleaning chemistry matters as much as polishing. Residues from aqueous detergents, solvent drying marks, and drag-out from ultrasonic baths each leave films measurable in monolayers. Good coating suppliers clean again before loading the chamber, but they clean better surfaces than they fix.
What to specify at the substrate level
- Glass material and manufacturer grade, with striae and bubble grade named.
- Used aperture explicitly, so bubble and striae limits apply where they matter.
- Transmitted wavefront requirement, not only surface flatness.
- Surface quality (scratch-dig) consistent with the wavelength: UV work needs tighter grades than visible.
- Polish method and final cleaning, if the coating is critical.
- Stress-birefringence limits for polarisation-sensitive paths.
Coatings get the attention because they are the last thing added and the first thing blamed. But the ceiling on a coated part's performance is set underneath the coating. Buyers who specify the substrate with the same rigour as the film are the ones whose parts match the datasheet.
Product page: optical glass blanks and windows — specifications, coating options and lead times.